Application:
E511 white light-proof films are produced using an advanced manufacturing process, and are known for their superior mechanical property, excellent electrical insulation, excellent resistance to water vapor, superior heat and humidity resistance, good tear resistance and coating property and other advantageous features. BOPET photovoltaic solar cell back films are produced by special slice and are primarily used as the base film for a photovoltaic solar cell back material.
Structure Chart of BOPET Photovoltaic Solar Cell Back Film:
A: Anti-adhesion layer
B: PET film with hydrolysis resistant
Properties | Unit | Typical value | Test Method | |||
Thickness | μm | 250 | 265 | 270 | ASTM D347 | |
Tensile Strength | MD | N/mm2 | 190 | 190 | 190 | ASTM 882 |
TD | N/mm2 | 210 | 210 | 210 | ||
Elongation at Break | MD | % | 180 | 180 | 180 | |
TD | % | 140 | 140 | 140 | ||
Thermal Shrinkage30Minute at 150℃ | MD | % | 0.8 | 0.8 | 0.8 | ASTM D1204 |
TD | % | |||||
Transmittance | % | 30 | 30 | 30 | ASTM D1003 | |
PCT48(121℃,100%RH) | % | >30 | >30 | >30 | GB/T13542.4-2009 | |
Electric Strength | KV/mm | >16 | >16 | >16 | GB/T13542.4-2009 | |
Partial discharge | VCD | >1000 | >1000 | >1000 | IEC61730-21-2004 | |
Wetting Tension | MN/m | 56 | 56 | 56 | ASTM D2578 |
The above data is the typical value of the BOPET film, which is for reference only rather than guaranteed value.